Breadcrumb

  • 【Organization】SAE
  • 【Document #】SAE AMS5853C
  • Steel, Corrosion and Heat-Resistant, Bars and Wire 15Cr - 25.5Ni - 1.2Mo - 2.1Ti - 0.006B - 0.30V Consumable Electrode Melted 1800 °F (982 °C) Solution Treated and Work-Strengthened 160 ksi (1103 MPa) Tensile Strength - UNS S66286

  • 【Date】2006/6/1
  • 【Reaffirmed Date】(R 2012)
  • 【Language】English
  • 【Status】Active
  • 【Organization】SAE
  • 【Document #】SAE AMS5737P
  • Steel, Corrosion and Heat-Resistant, Bars, Wire, Forgings, and Tubing 15Cr - 25.5Ni - 1.2Mo - 2.1Ti - 0.006B - 0.30V Consumable Electrode Melted 1650 °F (899 °C) Solution and Precipitation Heat Treated - UNS S66286

  • 【Date】2006/6/1
  • 【Reaffirmed Date】(R 2018)
  • 【Language】English
  • 【Status】Active
  • 【Organization】SAE
  • 【Document #】SAE AMS5737P
  • Steel, Corrosion and Heat-Resistant, Bars, Wire, Forgings, and Tubing 15Cr - 25.5Ni - 1.2Mo - 2.1Ti - 0.006B - 0.30V Consumable Electrode Melted 1650 °F (899 °C) Solution and Precipitation Heat Treated - UNS S66286

  • 【Date】2006/6/1
  • 【Reaffirmed Date】(R 2018)
  • 【Language】English
  • 【Status】Active
  • 【Organization】SAE
  • 【Document #】SAE AMS5734K
  • Steel, Corrosion and Heat-Resistant, Bars, Wire, Forgings, and Tubing 15Cr - 25.5Ni - 1.2Mo - 2.1Ti - 0.006B - 0.30V Consumable Electrode Melted, 1650 °F (899 °C) Solution Heat Treated - UNS S66286

  • 【Date】2006/6/1
  • 【Reaffirmed Date】(R 2018)
  • 【Language】English
  • 【Status】Active
  • 【Organization】SAE
  • 【Document #】SAE AMS5731L
  • Steel, Corrosion and Heat-Resistant, Bars, Wire, Forgings, Tubing, and Rings 15Cr - 25.5Ni - 1.2Mo - 2.1Ti - 0.006B - 0.30V Consumable Electrode Melted, 1800 °F (982 °C) Solution Heat Treated - UNS S66286

  • 【Date】2006/6/1
  • 【Reaffirmed Date】(R 2018)
  • 【Language】English
  • 【Status】Active
  • 【Organization】SAE
  • 【Document #】SAE AMS5897B
  • Steel, Corrosion and Heat-Resistant, Seamless or Welded Hydraulic Tubing 18.5Cr - 11Ni - 0.80Cb (Nb) (SAE 30347) Solution Heat Treated and Cold Drawn, 1/8 Hard Temper - UNS S34700

  • 【Date】2006/6/1
  • 【Reaffirmed Date】(R 2012)
  • 【Language】English
  • 【Status】Active
  • 【Organization】SAE
  • 【Document #】SAE AMS5591K
  • Steel, Corrosion and Heat-Resistant, Tubing, Seamless 12.5Cr (SAE 51410) Annealed - UNS S41000

  • 【Date】2006/6/1
  • 【Reaffirmed Date】(R 2012)
  • 【Language】English
  • 【Status】Active
  • 【Organization】SAE
  • 【Document #】SAE AMS5347B
  • Steel, Corrosion-Resistant, Investment Castings 15Cr - 4.6Ni - 0.22Cb (Nb) - 2.8Cu Solution and Precipitation Heat Treated (H1000) 150 ksi (1034 MPa) Tensile Strength (15-5) - UNS J92110

  • 【Date】2006/6/1
  • 【Reaffirmed Date】(R 2014)
  • 【Language】English
  • 【Status】Active
  • 【Organization】SAE
  • 【Document #】SAE AMS5346C
  • Steel, Corrosion-Resistant, Investment Castings 15Cr - 4.6Ni - 0.22Cb (Nb) - 2.8Cu Solution and Precipitation Heat Treated (H925) 180 ksi (1241 MPa) Tensile Strength (15-5) - UNS J92110

  • 【Date】2006/6/1
  • 【Reaffirmed Date】(R 2014)
  • 【Language】English
  • 【Status】Active
  • 【Organization】SAE
  • 【Document #】SAE AMS5342E
  • Steel, Corrosion-Resistant, Investment Castings 16Cr - 4.1Ni - 0.28Cb (Nb) - 3.2Cu Homogenization, Solution, and Precipitation Heat Treated (H1100) 130 ksi (896 MPa) Tensile Strength (17-4) - UNS J91280 and UNS J92200

  • 【Date】2006/6/1
  • 【Reaffirmed Date】(R 2014)
  • 【Language】English
  • 【Status】Active